Gold platinum ceramic alloy in compliance with DIN EN ISO 9693 +
DIN EN ISO 22674. Type 4, pale yellow, palladium-free, copper-free.

Matching solders

Investment material: Phosphate-bonded
Casting crucible: Graphite / ceramic

Post melting time in seconds

  • Resistance heating: 60 - 120
  • HF induction: 5 - 15
  • Propane / oxygen flame: 5 - 15

Oxidation without vacuum, ºC/min: 930 / 5 
Tempering, °C/min: 550 / 15 
Soft annealing, ºC/min: -

Porta Impulsmagnifying glass

Composition
Au 61.0
Pt 28.0
Ag 7.0
Zn 1.5
Cu 1.0
In 1.0
Ir < 1.0

The recommended solders for this alloy
Solder befor firing: Porta IP Lot V-1
Solder after firing: Porta OP Lot W-2
Laser-welding wires: Porta Geo Ti